Tape casting and its characterization for Sr0.65La0.35Ti0.65Co0.35O 3

dc.contributor.authorKumar D.; Upadhyay S.; Parkash O.
dc.date.accessioned2025-05-24T09:57:13Z
dc.description.abstractProcedure of tape casting by the doctor blade method for Sr0.65La0.35Ti0.65Co0.35O 3 which shows maximum value of dielectric constant in the system Sr1-xLaxTi1-xCoxO3 (0.20 ≤ x ≤ 0.40) has been described. Dielectric behaviour and microstructure of the tape have been studied.
dc.identifier.doihttps://doi.org/10.1016/S0167-577X(97)00022-0
dc.identifier.urihttp://172.23.0.11:4000/handle/123456789/21910
dc.relation.ispartofseriesMaterials Letters
dc.titleTape casting and its characterization for Sr0.65La0.35Ti0.65Co0.35O 3