Repository logo
Institutional Digital Repository
Shreenivas Deshpande Library, IIT (BHU), Varanasi

Sintering studies of equimolar mgo-cao-ai2o3 mix

dc.contributor.authorSharma S.C.; Ali M.M.; Agrawal G.N.
dc.date.accessioned2025-05-24T09:55:39Z
dc.description.abstractThe kinetics and densification study of the equimolar mix of MgO-CaO-AI2O3 at 1275°, 1300° and 1340°C indicated significant change in densification only at 1340°C. At 1275° and 1300°C, no densification was observed and the fired bulk density was found to be lower than the green bulk density. However, at 1340°C, considerable densification was observed due to sintering effect even in 15 min and maximum densification was seen in 7 h. The volume decrease observed on sintering was found to be 50.74%, which was accompanied with the formation of a small amount of calcium aluminate phases. The activation energy for densification of the optimum composition was found to be 79.4 kcal/mole. The optimised equimolar composition of MgO, CaO and AI2O3 which attained maximum densification at 1340°C in 7 h, showed apparent porosity, cold crushing strength and fusion temperature values of 1.82%, 2890 kg.cm−2 and 1498°C respectively. © 2003 Taylor and Francis Group, LLC.
dc.identifier.doihttps://doi.org/10.1080/0371750X.2003.11012066
dc.identifier.urihttp://172.23.0.11:4000/handle/123456789/20094
dc.relation.ispartofseriesTransactions of the Indian Ceramic Society
dc.titleSintering studies of equimolar mgo-cao-ai2o3 mix