Repository logo
Institutional Digital Repository
Shreenivas Deshpande Library, IIT (BHU), Varanasi

Comparative Dielectric and Ferroelectric Characteristics of Bi0.5Na0.5TiO3, CaCu3Ti4O12, and 0.5Bi0.5Na0.5TiO3–0.5CaCu3Ti4O12 Electroceramics

Loading...
Thumbnail Image

Date

Journal Title

Journal ISSN

Volume Title

Publisher

Abstract

Abstract: The dielectric and ferroelectric characteristics of Bi0.5Na0.5TiO3 (BNT), CaCu3Ti4O12 (CCTO), and 0.5Bi0.5Na0.5TiO3–0.5CaCu3Ti4O12 (BNT/CCTO) ceramics are compared. X-ray diffraction patterns confirmed the formation of single phase of all the ceramics after sintering at 950°C for 15 h. Scanning electron microscopy images of the sintered ceramics reveal average grain sizes in the range from 200 nm to 2.5 μm. Energy-dispersive x-ray mapping and x-ray photoelectron spectroscopy show the presence of the elements Bi, Na, Ca, Cu, Ti, and O with uniform distribution in the ceramics. BNT/CCTO exhibits high dielectric constant (εr ∼ 6.9 × 104) compared with BNT (εr ∼ 0.13 × 104) and CCTO (εr ∼ 1.68 × 104) ceramics at 1 kHz and 503 K. The high dielectric constant of BNT/CCTO compared with BNT and CCTO is associated with a major contribution from grain boundaries, as confirmed by impedance and modulus analyses. The P–E hysteresis loop of all the ceramics measured at room temperature and 50°C exhibited typical ferroelectric nature. The remanent polarization (Pr) of BNT (1.58 μC/cm2) and CCTO (0.654 μC/cm2) ceramics are higher than that of BNT/CCTO (0.267 μC/cm2) ceramic. Graphical Abstract: [Figure not available: see fulltext.] © 2016, The Minerals, Metals & Materials Society.

Description

Keywords

Citation

Collections

Endorsement

Review

Supplemented By

Referenced By