Influence of calcination and sintering temperatures on the structure of (Pb1-xBax)ZrO3

dc.contributor.authorPokharel B.P.; Datta M.K.; Pandey D.
dc.date.accessioned2025-05-24T09:55:16Z
dc.description.abstract(Pb1-xBax)ZrO3 powders are synthesized below 800°C for x ≤ 0.25 using a semi-wet route involving solid-state thermochemical reaction in a mixture of ZrO2 and (Pb1-xBax)CO3. The (Pb1-xBax)CO3 precursors were obtained by a 'forced' coprecipitation technique. These powders can be sintered to achieve nearly 99% of the theoretical density at 1050°C, which is 200 to 300°C lower than that employed for the solid state route. The structure of as-calcined powder is orthorhombic for x ≤ 0.10 and rhombohedral for 0.25 < x ≤ 0.35, whereas the two phases coexist for 0.15 ≤ x ≤ 0.25. The structure of sintered material is orthorhombic for 0 ≤ x ≤ 0.10, rhombohedral for 0.20 ≤ x ≤ 0.30, and cubic for x ≥ 0.35, whereas orthorhombic and rhombohedral phases coexist at x = 0.15. The difference in the structure of the as-calcined and sintered powders is discussed in terms of particle size effect and chemical homogenisation of Ba2+ in the PBZ matrix.
dc.identifier.doihttps://doi.org/10.1023/A:1004552308815
dc.identifier.urihttp://172.23.0.11:4000/handle/123456789/19661
dc.relation.ispartofseriesJournal of Materials Science
dc.titleInfluence of calcination and sintering temperatures on the structure of (Pb1-xBax)ZrO3