Solvothermal synthesis of high value copper powder from copper bleed solution of an Indian copper smelter
| dc.contributor.author | Meshram P.; Sinha M.K.; Sahu S.K.; Khan P.; Pandey B.D.; Mankhand T.R. | |
| dc.date.accessioned | 2025-05-24T09:18:16Z | |
| dc.description.abstract | Recovery of copper powder from copper bleed solution (CBS) of a copper smelter by solvothermal route has been investigated. After removing sulphuric acid by solvent extraction with tri-iso-octyl-amine, copper from the acid depleted CBS was recovered by using Versatic 10 acid as an extractant in kerosene. In 1.5. M Versatic 10 acid 29.8. g/L copper was loaded at an equilibrium pH of 4.25. During the hydrogen stripping, a 97% copper powder was recovered from the loaded Versatic 10 acid solution at 20. bar hydrogen pressure and 403. K temperature. The solvothermal synthesis of copper powder followed nucleation and growth kinetic model with activation energy value of 145. kJ/mol. Stripping of copper powder could also follow the chemical control kinetic model with lower value of activation energy (66. kJ/mol). The copper powder as characterized by SEM exhibited globular particles of 0.25-0.5 μm size and was found to be suitable for P/M applications. © 2012 Elsevier B.V. | |
| dc.identifier.doi | https://doi.org/10.1016/j.powtec.2012.07.049 | |
| dc.identifier.uri | http://172.23.0.11:4000/handle/123456789/13983 | |
| dc.relation.ispartofseries | Powder Technology | |
| dc.title | Solvothermal synthesis of high value copper powder from copper bleed solution of an Indian copper smelter |