Synthesis of Fe-Si-B-Mn-based nanocrystalline magnetic alloys with large coercivity by high energy ball milling

dc.contributor.authorReddi, P.D.
dc.contributor.authorMukhopadhyay, N.K.
dc.contributor.authorMajumdar, B.
dc.contributor.authorSingh, A.K.
dc.contributor.authorMeena, S.S.
dc.contributor.authorYusuf, S.M.
dc.contributor.authorPrasad, N.K.
dc.date.accessioned2021-10-18T05:07:42Z
dc.date.available2021-10-18T05:07:42Z
dc.date.issued2014-06
dc.description.abstractAlloys of Fe-Si-B with varying compositions of Mn were prepared using high energy planetary ball mill for maximum duration of 120 h. X-ray diffraction (XRD) analysis suggests that Si gets mostly dissolved into Fe after 80 h of milling for all compositions. The residual Si was found to form an intermetallic Fe3Si. The dissolution was further confirmed from the field emission scanning electron microscopy/energy dispersive X-ray analysis (FE-SEM/EDX). With increased milling time, the lattice parameter and lattice strain are found to increase. However, the crystallite size decreases from micrometer (75-95 μm) to nanometer (10-20 nm). Mössbauer spectra analysis suggests the presence of essentially ferromagnetic phases with small percentage of super paramagnetic phase in the system. The saturation magnetization (Ms), remanance (Mr) and coercivity (Hc) values for Fe-0Mn sample after 120 h of milling were 96·4 Am2/kg, 11·5 Am2/kg and 12·42 k Am -1, respectively. However, for Fe-10Mn-5Cu sample the Ms, Hc and Mr values were found to be 101·9 Am 2/kg, 10·98 kA/m and 12·4 Am2/kg, respectively. The higher value of magnetization could be attributed to the favourable coupling between Mn and Cu.en_US
dc.description.sponsorshipBulletin of Materials Scienceen_US
dc.identifier.issn02504707
dc.identifier.urihttps://idr-sdlib.iitbhu.ac.in/handle/123456789/1803
dc.language.isoenen_US
dc.publisherIndian Academy of Sciencesen_US
dc.relation.ispartofseriesIssue 4;Volume 37
dc.subjectAmorphization;en_US
dc.subjectLattice strain;en_US
dc.subjectMagnetic properties;en_US
dc.subjectMechanical alloyingen_US
dc.titleSynthesis of Fe-Si-B-Mn-based nanocrystalline magnetic alloys with large coercivity by high energy ball millingen_US
dc.typeArticleen_US

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Synthesis-of-FeSiBMnbased-nanocrystalline-magnetic-alloys-with-large-coercivity-by-high-energy-ball-millingBulletin-of-Materials-Science.pdf
Size:
759.07 KB
Format:
Adobe Portable Document Format
Description:
Experimental

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description: