Effect of dopants on high alumina ceramic materials
| dc.contributor.author | Sharma L.K.; Agrawal G.N.; Josm V.C. | |
| dc.date.accessioned | 2025-05-24T09:58:41Z | |
| dc.description.abstract | Investigations were carried out on the effect of dopants on the sintering behaviour of high alumina ceramics. The dopants were Ti02, Sn02 and (Ti02+Sn02). The effects of different dopants, viz. 1, 3 and S wt% of Ti02, Sn02 and (Ti02 1+SnO,) on the sintering of alumina were studied at various temperatures (1300°, 1400°, 1450° and 1600T) and soaking times (10, 30, 50, 100 and 150 mins). The study revealed that 5 wt% of (TiOd+SnO,) gave the maximum densification at 1600°C and 150 mins soaking period. © 1986 Taylor & Francis Group, LLC. | |
| dc.identifier.doi | https://doi.org/10.1080/0371750X.1986.10822779 | |
| dc.identifier.uri | http://172.23.0.11:4000/handle/123456789/23584 | |
| dc.relation.ispartofseries | Transactions of the Indian Ceramic Society | |
| dc.title | Effect of dopants on high alumina ceramic materials |